Pmullen503 wrote:Resin and glass isn't than much more expensive than PMF and is more waterproof.
I did the numbers on PMF over Fiberglassing just to see what the price difference really is. People always say that fiberglassing is just a little bit more than PMF so why not just Fiberglass. Well, there really is a reason it is called PMF.
Here are the numbers using the materials recommended earlier in this post for fiberglassing.
6 Yards 6oz x 60" Fiberglass $46.50
6 Yards 6oz x 50" Fiberglass $42.00
6 qt Kit Non-Blushing Epoxy $114.05
Total Before Shipping Costs and Tax $202.55
Here are the numbers for PMF.
15 Yards 60" 7 oz Cotton Duck $59.85
1 Gal Tight Bond II $26.99
Total Before Shipping Costs and Tax $86.84
I did not add in tax and shipping because that is a variable that might be mitigated by local resources. If you did however have to order in the materials the epoxy resin and fiberglass is 37.04 for shipping. I would suspect that is because it is a chemical. 15 yards of cotton duck cost 7.99 for shipping. Tight Bond II is available everywhere, so I did not include a shipping cost for it.
In this case the cost difference of PMF over fiberglassing is nearly 1/3 the cost. The larger the project the bigger the cost difference would be.
I have use fiberglass and I don't like working with it. Nothing about it is fun to me. PMF just works and it is simple to do. I always tell people, if you can hang wall paper you can PMF. You also don't have to worry about a possible reaction to it.
As far as fiberglass being more waterproof? I doubt it. Here are some pictures of TBII that I had thinned down to 50/50. 50/50 is my go to mix ratio for all my builds.
Now imagine TBII applied to the wood then canvas and then another coat of TBII. It is going to be watertight.
Well, that is my two cents... Carry on.