Step 15: Skin the exterior- Uniflex255

Step 15: Skin the exterior- Uniflex255
There are a number of different ways to skin the exterior, aluminum, filon, pvc and more. I chose to paint the exterior with Uniflex255, a boat hull paint from the rot doctor. I figured if it was good enough for boat hulls, it was good enough for the teardrop.
The rot doctor recommends treating all surfaces with CPES before patching or painting. The CPES is a thinned out epoxy that penetrates into the grain of the wood, and hardening, creating a tough, durable seal, and will prevent the wood from rotting.
Once the CPES is dry (at least several hours), the next step is to patch all holes and defects with Fill it Epoxy Filler.
Let the Fill-It Epoxy filler cure overnight.
The next day use a combination of belt sander and random orbital sander to sand all that Filler smooth.
Finally mix up your Uniflex 255 and apply with a solvent resistant roller.


There are a number of different ways to skin the exterior, aluminum, filon, pvc and more. I chose to paint the exterior with Uniflex255, a boat hull paint from the rot doctor. I figured if it was good enough for boat hulls, it was good enough for the teardrop.
The rot doctor recommends treating all surfaces with CPES before patching or painting. The CPES is a thinned out epoxy that penetrates into the grain of the wood, and hardening, creating a tough, durable seal, and will prevent the wood from rotting.

Once the CPES is dry (at least several hours), the next step is to patch all holes and defects with Fill it Epoxy Filler.

Let the Fill-It Epoxy filler cure overnight.
The next day use a combination of belt sander and random orbital sander to sand all that Filler smooth.

Finally mix up your Uniflex 255 and apply with a solvent resistant roller.