by ZendoDeb » Wed May 20, 2009 9:15 pm
West System
System 3
System 3 Silver Tip
MAS
I have also used the house brand from Fiberglass Coatings.
Sources: Fiberglass Coatings, Jamestown Distributors, Boatbuilder Central, etc.
Things to consider with epoxy:
Epoxy doesn't have a lot of UV protection. Cover it with a clear-coat auto-finish like Imron or Alwgrip.
The slower the cure, the harder the finished product.
The more resin/hardener the harder the finished product.
West System is 5 to 1 - very hard, difficult to mix in small quantities (buy the mixing pumps)
Most of the others are going to be 2 to 1 or even 1 to 1.
Stay away from 5 minute epoxies EXCEPT to tack things in place for later lamination using real epoxy.
Jamestown Distributors also sells a laminating epoxy from Smiths (the people who make CPES) but I can't find any strength-test data on it.
"Houses are but badly built boats so firmly aground that you cannot think of moving them.... The desire to build a house is the tired wish of a man content thenceforward with a single anchorage. The desire to build a boat is the desire of youth, unwilling yet to accept the idea of a final anchorage." - Arthur Ransome: Racundra's First Cruise, 1923